权利要求:
We claim:
1. An article, comprising:
a biofabricated leather material in a design or pattern and/or a biofabricated material present on a substrate in a design or pattern.
2. The article of claim 1, wherein the biofabricated material adheres to a second
material.
3. The article of claim 2, wherein the second material is selected from the group
consisting of a second biofabricated leather material and a fabric.
4. The article of claim 3, wherein the fabric is natural, synthetic or both.
5. The article of claim 3, wherein the fabric is selected from the group consisting of woven, non- woven, a knit and a combination thereof.
6. The article of claim 1, wherein the biofabricated leather material comprises
recombinant bovine collagen.
7. The material of claim 1 , wherein the design or pattern is a lace-like design or pattern.
8. An article comprising:
one or more materials with opposing edges and a gap between the edges; and a biofabricated leather material that fills the gap and overlaps the opposing edges to bond the opposing edges of the material.
9. The article of claim 8, wherein the material is a biofabricated leather material, a fabric, or a combination thereof.
10. The article of claim 9, wherein the material is a fabric and the fabric is natural,
synthetic or a combination thereof.
11. The article of claim 9, wherein the material is a fabric and the fabric is woven, non- woven, a knit or a combination thereof.
12. The article of claim 9, wherein the material is a fabric and the fabric comprises fibers, the fibers being protein, cellulose, or a combination thereof and wherein the edges of the fabric are devored.
13. The article of claim 8, wherein the biofabricated leather material comprises
recombinant bovine collagen.
14. An article comprising:
a material pretreated with a solution; and
a biofabricated leather material in a design or pattern bonded to the material.
15. The article of claim 14, wherein the material is a cellulose fabric pretreated with a periodate solution.
16. The article of claim 15, wherein the cellulose fabric is selected from the group
consisting of viscose, acetate, lyocell, bamboo and a combination thereof.
17. The article of claim 15, wherein the periodate pretreatment includes 25% to 100% periodate by weight of the fabric.
18. The article of claim 15, wherein the periodate pretreatment comprises exposing the fabric to the periodate solution for 15 mins to 24 hours, quenching the periodate with a glycol, rinsing the fabric with water and drying the fabric.
19. The article of claim 18, wherein the glycol is selected from the group consisting of ethylene glycol, propylene glycol, diethylene glycol, dipropylene glycol, triethylene glycol, polyethylene glycol, butylene glycol and a combination thereof.
20. The article of claim 14, wherein the material is a fabric pretreated with a collagen solution.
21. The article of claim 20, wherein the fabric is selected from the group consisting of natural, synthetic and a combination thereof.
22. The article of claim 21, wherein the fabric is selected from the group consisting of woven, non- woven, knit and a combination thereof.
23. The article of claim 20, wherein the collagen pretreatment comprises applying a 0.5 mg/ml to 10 mg/ml collagen solution to the fabric.
24. The article of claim 14, wherein the collagen pretreatment comprises pouring a
collagen solution into a container, cooling the container, mixing the solution, adding a buffer to the solution to induce fibrillation, filtering the solution through the fabric, placing the fabric and the filtrate in the container and mixing.
25. A method of making a biofabricated leather bonded article, the method comprising: placing a material having opposed edges on a surface wherein there is a gap between the opposed edges; applying an aqueous solution of collagen in the gap between the opposed edges to fill the gap and overlap the opposing edges, the aqueous solution of collagen optionally comprising a binder; and drying to form the biofabricated leather bonded article.
26. The method of claim 25, wherein the material is a biofabricated leather material, a fabric, or both.
27. The method of claim 26, wherein the material is a fabric that is natural, synthetic or a combination thereof.
28. The method of claim 26, wherein the material is a fabric that woven, non- woven, a knit or a combination thereof.
29. The method of claim 26, wherein the material is a fabric that has a mesh ranging from 300 threads per square inch to 1 thread per square foot or a pore size greater than or equal to 1 1 μιη in diameter.
30. The method of claim 26, wherein the material is a fabric that is pretreated to improve collagen bonding.
31. The method of claim 30, wherein the pretreatment comprises applying a collagen solution comprising 0.5 mg/ml to 10 mg/ml of collagen to the fabric.
32. The method of claim 31, wherein the collagen pretreatment comprises pouring a collagen solution into a container, cooling the container, mixing the solution, adding a buffer to the solution to induce fibrillation, filtering the solution through the fabric, placing the fabric and the filtrate in the container and mixing.
33. The method of claim 30, wherein the pretreatment comprises applying a periodate solution to a cellulose fabric.
34. The method of claim 25, wherein the biofabricated leather bonded material comprises recombinant bovine collagen.
35. The method of claim 25, wherein the drying comprises vacuum, heated air drying, ambient air drying, heated pressing, pressure drying and a combination thereof.
36. The method of claim 35, wherein the drying comprises a vacuum with a pressure of from 0 to 14 psi.
37. The method of claim 25, wherein the biofabricated leather fabric is dried for 30
minutes to 24 hours.
38. The method of claim 25, wherein the biofabricated leather fabric is dried at a
temperature of from about 20°C to 80°C.
39. The article of claim 1 , wherein the biofabricated leather material is made from an aqueous fibrillated cross-linked collagen solution.
40. The article of claim 1, wherein the biofabricated leather material is made from an aqueous fibrillated cross-linked collagen solution and the solution is deposited by pouring, pipetting, with a nozzle, or other liquid deposition means.
41. The article of claim 40, wherein the solution is deposited in an automated deposition system.
42. The article of claim 40, wherein the biofabiicated leather material creates a texture on the substrate.
43. The method of claim 25, wherein the aqueous solution of collagen is applied on the material is a pattern or design.
44. The method of claim 25, wherein the aqueous solution of collagen is applied by liquid deposition techniques selected from the group consisting of pouring, pipetting, with a nozzle, marquetry, paletting, and combinations thereof.
45. The method of claim 44, wherein the solution is deposited in an automated deposition system.
46. The method of claim 25, wherein the material has been treated to create one or more holes or voids.
47. The method of claim 46, wherein the aqueous solution of collagen is applied to the one or more holes or voids
48. The method of claim 46, wherein the one or more holes or voids are created by
selectively removing a portion of the material physically, chemically, or by burning.
49. The article of claim 8, wherein the opposing edges that are bonded by the
biofabricated leather material are edges of a single continuous material.
50. The article of claim 8, wherein the opposing edges that are bonded by the
biofabricated leather material are edges on two or more different non-continuous materials.
51. The article of claim 50, wherein the two or more different materials have the same or substantially the same composition.
52. The article of claim 50, wherein the two or more different materials have different compositions.
53. The article of claim 1, wherein the design or pattern is raised to impart a three dimensional texture.
54. An article, comprising:
a three-dimensional object having biofabricated leather material on a surface thereof.
55. The article of claim 54, wherein the biofabricated leather material is applied by liquid deposition techniques selected from the group consisting of dipping, pouring, pipetting, with a nozzle, marquetry, paletting, and combinations thereof.
56. The article of claim 54, wherein the three-dimensional object is printed.
57. The article of claim 56, wherein the three-dimensional object comprises
photopolymer resin.